- A Mete, Y Yilmaz, and S S Derelioglu.
- Department of Pediatric Dentistry, Faculty of Dentistry, Ataturk University, Erzurum, Turkiye.
- Niger J Clin Pract. 2018 Apr 1; 21 (4): 525-530.
AbstractPurpose: To compare fracture resistance force (FRF) and failure types of crowns milled from resin nanoceramic (Lava Ultimate)-, and modified polymethylmethacrylate (PMMA) (Vita computer-aided design (CAD)-Temp)-, and PMMA (Telio CAD)-based CAD/computer-assisted manufactured (CAM) blocks. Materials and Methods: Three experimental groups of 10 milled crowns were arranged: Group-1 (Lava Ultimate), Group-2 (Vita CAD-Temp), and Group-3 (Telio CAD). Crowns were machined in sizes similar to a primary second molar stainless steel crown (SSC) and stored in water at 37°C for 30 days. The crowns were seated on Cr-Co dies. Their FRFs were measured using a universal test machine until fracture. FRFs and failure types were recorded and statistically analyzed (P < 0.05). Results: There were statistically significant differences among the groups for both FRFs and failure types. The sources of significant differences for FRFs and failure types were Group-3 and Group-1, respectively.
Notes
Knowledge, pearl, summary or comment to share?You can also include formatting, links, images and footnotes in your notes
- Simple formatting can be added to notes, such as
*italics*
,_underline_
or**bold**
. - Superscript can be denoted by
<sup>text</sup>
and subscript<sub>text</sub>
. - Numbered or bulleted lists can be created using either numbered lines
1. 2. 3.
, hyphens-
or asterisks*
. - Links can be included with:
[my link to pubmed](http://pubmed.com)
- Images can be included with:
![alt text](https://bestmedicaljournal.com/study_graph.jpg "Image Title Text")
- For footnotes use
[^1](This is a footnote.)
inline. - Or use an inline reference
[^1]
to refer to a longer footnote elseweher in the document[^1]: This is a long footnote.
.