Proceedings of the Institution of Mechanical Engineers. Part H, Journal of engineering in medicine
-
Proc Inst Mech Eng H · Jan 2000
ReviewBiological reactions to wear debris in total joint replacement.
The vast majority of total hip prostheses currently implanted consist of a hard metal or ceramic femoral head articulating against an ultra-high molecular weight polyethylene (UHMWPE) acetabular cup. Over the last 10 years, evidence has accumulated to show that these prostheses are prone to failure due to late aseptic loosening and few survive beyond 25 years. With an increasing need to implant hip prostheses in the younger, more active patient the need to understand the mechanisms of failure and to develop artificial hip joints using alternative materials have become major issues in the orthopaedic community. ⋯ For metal-on-metal prostheses, the prospects for increasing the osteolysis free life of the implant are good but additional biological problems associated with the nanometre size and reactivity of the wear particles in vivo may emerge. For the ceramic-on-ceramic prostheses, although initial prospects are encouraging, more data are needed on the characteristics of the wear particles generated in vivo before predictions can be made. It is concluded that the pre-clinical testing of any new materials for joint replacement must include an analysis of the wear particle characteristics and their biological reactivity in addition to the usual assessment of wear.
-
Proc Inst Mech Eng H · Jan 2000
Comparative StudyA comparative joint simulator study of the wear of metal-on-metal and alternative material combinations in hip replacements.
While total hip replacement represents the major success story in orthopaedic surgery in the twentieth century, there is much interest in extending even further, early in the twenty first century, the life of implants. Osteolysis has been identified as a major factor limiting the life of prostheses, with indications that fine polyethylene wear debris, generated primarily at the interface between the femoral head and the acetabular cup, promotes the process. There is therefore considerable interest in the introduction of alternative wear resistant systems to limit the deleterious effects of wear. ⋯ The number of metallic particles may exceed the number of polyethylene wear particles from an otherwise similar metal-on-polyethylene joint by a factor of 10(3). A detailed discussion of the size and morphology of wear debris and tissue reaction to various forms of debris is beyond the scope of this paper, but the biological response to polymeric, metallic and ceramic wear debris forms a major subject for further study. The present investigation nevertheless confirms the potential of carefully designed and manufactured metal-on-metal total replacement joints for the treatment of diseased and damaged hips.